description
Loading Density: 30%-70% (Fe3O4 nanocrystal) by TEM
Resistance: <103 Ω/sq (graphene)
form
dispersion
composition
acetone, ~80 wt. %
Fe3O4 nanoparticle, 4-9%
graphene, 3-8%
concentration
10 mg/mL in acetone
thickness
1-10 nm , graphene
particle size
5-25 nm (Fe3O4 nanocrystal)
storage temp.
2-8°C
Application
- Electromagnetic wave absorption materials.
- Electro-magnetic device.
- Anode material for lithium-ion batteries.
Legal Information
signalword
Danger
hcodes
Hazard Classifications
Eye Irrit. 2 - Flam. Liq. 2 - STOT SE 3
target_organs
Central nervous system
supp_hazards
Storage Class
3 - Flammable liquids
wgk_germany
WGK 3
flash_point_f
59.0 °F
flash_point_c
15 °C
Choose from one of the most recent versions:
Certificates of Analysis (COA)
Don't see the Right Version?
If you require a particular version, you can look up a specific certificate by the Lot or Batch number.
Already Own This Product?
Find documentation for the products that you have recently purchased in the Document Library.
Our team of scientists has experience in all areas of research including Life Science, Material Science, Chemical Synthesis, Chromatography, Analytical and many others.
Contact Technical Service